MATERIAL |
MWS-650 |
|
|
CHEMICAL COMPOSITION (%) |
80 Ni, 20 Cr |
|
|
RESISTIVITY AT 20°C |
OHMS/CMF |
650 |
|
TCR 0-100°C |
.00010 |
|
|
COEFFICIENT OF LINEAR EXPANSION
BETWEEN 20-100°C |
.0000132 |
|
|
TENSILE STRENGTH |
MIN. |
100,000 |
|
MAX. |
200,000 |
|
|
SPECIFIC GRAVITY |
8.412 |
|
|
POUNDS PER CUBIC INCH |
.3039 |
|
|
MAGNETIC ATTRACTION |
None |
|
|
APPROX. MELTING POINT (°C) |
1400 |
|
|
MINIMUN
QUANTITY ORDER: 10LB |
||




(0.00)stars out of 5