MATERIAL |
MWS-675 |
|
|
CHEMICAL COMPOSITION (%) |
61 Ni, 15 Cr, bal. Fe |
|
|
RESISTIVITY AT 20°C |
OHMS/CMF |
675 |
|
TCR 0-100°C |
.00013 |
|
|
COEFFICIENT OF LINEAR EXPANSION
BETWEEN 20-100°C |
0000137 |
|
|
TENSILE STRENGTH |
MIN. |
95,000 |
|
MAX. |
175,000 |
|
|
SPECIFIC GRAVITY |
8.247 |
|
|
POUNDS PER CUBIC INCH |
.2979 |
|
|
MAGNETIC ATTRACTION |
Faint |
|
|
APPROX. MELTING POINT (°C) |
13 |
|
|
MINIMUN
QUANTITY ORDER: 10LB |
||